ISO 3834: comprehensive, standard and elementary requirements
ISO 3834 sets quality requirements for fusion welding in the workshop, not for a single weld. Part 2 is the comprehensive level, part 3 the standard level and part 4 the elementary one. The three share one list of elements; the higher the part, the more of them are required and the more has to be written down.
Short answer
Part 2 — comprehensive, part 3 — standard, part 4 — elementary. Parts 2 and 3 both ask for a welding coordinator, WPS and procedure qualification; part 4 asks for neither. Part 2 adds records and plans that part 3 only recommends. Under EN 1090-2 the part follows the execution class: EXC1 — part 4, EXC2 — part 3, EXC3 and EXC4 — part 2. A manufacturer that meets a higher part is taken to meet the lower ones.
The ISO 3834 series
- Part 1 — criteria for choosing the level.
- Part 2 — comprehensive quality requirements.
- Part 3 — standard quality requirements.
- Part 4 — elementary quality requirements.
- Part 5 — the documents (standards) a manufacturer follows to claim conformity with part 2, 3 or 4.
- ISO/TR 3834-6 — guidance on implementation.
The series applies to the manufacturer, in the workshop and on site; it is not a personal certificate and says nothing about a single weld. The European adoption is EN ISO 3834.
Which part to choose
Product standards, regulations or the contract often name the part: EN 1090-2 does, by execution class (table below). Where nothing is named, part 1 gives the criteria: how safety-critical the products are, how complex the manufacture is, how wide the range of products and materials, how likely metallurgical problems are, and how far a manufacturing imperfection affects performance. As a guide, part 2 suits safety-critical products and complex manufacture, part 3 a medium level of both, part 4 products that are not safety-critical and routine processes. A manufacturer that meets part 2 meets parts 3 and 4 without further proof.
Requirements by part
The list of elements is the same in all three parts; what changes is whether an element is required, only recommended or absent. Read the table row by row.
| Element | Part 2 — comprehensive | Part 3 — standard | Part 4 — elementary |
|---|---|---|---|
| Review of requirements and technical review | record required | review required; record may be required | record not required |
| Sub-contracting | sub-contracted work treated as the manufacturer’s own; final responsibility stays with the manufacturer | as part 2 | as part 2 |
| Welders and welding operators | qualification required | qualification required | qualification required |
| Welding coordination personnel | required | required | no specific requirement |
| Inspection and testing personnel | qualification required | qualification required | qualification required |
| Equipment: suitable and available | required | required | required |
| Equipment maintenance | documented plans and records required | records recommended | no specific requirement |
| Description of equipment | list required | list required | no specific requirement |
| Production planning | required; documented plans and records required | required; records recommended | no specific requirement |
| Welding procedure specifications (WPS) | required | required | no specific requirement |
| Qualification of the welding procedures | required | required | no specific requirement |
| Batch testing of consumables | if required | no specific requirement | no specific requirement |
| Storage and handling of consumables | procedure required, following the supplier | following the supplier | following the supplier |
| Storage of parent material | protection from the environment; identification kept | protection from the environment; identification kept | no specific requirement |
| Post-weld heat treatment | own clause | own clause | no clause |
| Inspection and testing | own clause | own clause | own clause |
| Non-conformance and corrective actions | own clause | own clause | own clause |
| Calibration and validation of equipment | own clause | own clause | no clause |
| Identification and traceability | own clause | own clause | no clause |
| Quality records | own clause | own clause | own clause |
The last six rows show only whether the part has a clause on the subject. Inside a clause, parts 2 and 3 differ in depth, so the standard itself decides. Subcontractors are controlled in every part; the manufacturer keeps evidence of their compliance, for example a list with capabilities, audit reports or third-party certificates.
ISO 3834 and EN 1090
EN 1090-2 does not leave the part open:
| EN 1090-2 class | ISO 3834 part | Level of requirements |
|---|---|---|
| EXC1 | part 4 | elementary |
| EXC2 | part 3 | standard |
| EXC3 | part 2 | comprehensive |
| EXC4 | part 2 | comprehensive |
The FPC system of EN 1090-1 includes the welding quality system, so the ISO 3834 part is audited together with the rest of the factory production control by a notified body. Class, coordinator, procedure routes and quality levels: EN 1090 and the classes EXC1–EXC4.
The coordinator and ISO 14731
Welding coordination is the key idea of parts 2 and 3. The manufacturer defines the tasks and responsibilities of the coordination team on the basis of ISO 14731, and the people concerned must have the knowledge for the products and the chosen level: IWE, IWT or IWS qualifications are accepted as evidence when their level matches the production. Part 4 has no specific requirement for coordination, but someone still has to answer for the welding. The coordinator is also who signs the WPS and relies on the WPQR.
What an audit looks at
- the review of the order: which class, which materials, which standards;
- a current WPS for every joint in production and the WPQR behind it;
- welder certificates with valid confirmations;
- equipment lists, maintenance and calibration records where the part asks for them;
- consumable storage and the way they are handled;
- identification of material and welds and the quality records.
Standards and sources
- ISO 3834-1:2021, Annex A — criteria table for parts 2, 3 and 4 (preview pages, iTeh Standards).
- ISO 3834-2, -3, -4 — tables of contents of the previews (ISO, SIS, iTeh); clause numbers as in the 2005 editions, which the 2021 editions follow in structure.
- IIW, document IAB-337, «Interpretation and implementation of ISO 3834 requirements» — selection criteria, subcontractors, coordination.
- TWI, Job Knowledge 120 (twi-global.com) — the part required by EN 1090-2 for each class.
Frequently asked questions
What is the difference between ISO 3834-2, -3 and -4?
The level of requirements for the manufacturer’s welding quality system: part 2 comprehensive, part 3 standard, part 4 elementary. Parts 2 and 3 require a welding coordinator, WPS and qualified procedures; part 4 does not. Details in the table.
Which ISO 3834 part does EN 1090 require?
EXC1: part 4. EXC2: part 3. EXC3 and EXC4: part 2. See EN 1090 and EXC1–EXC4.
Is ISO 3834 a certificate for a welder?
No. It applies to the manufacturer and its quality system. Welders are tested separately to ISO 9606-1 (welder qualification), and the procedure is proved by a WPQR.
Does a part 2 certificate cover parts 3 and 4?
Yes. ISO 3834-1 says a manufacturer that meets a higher level meets the lower ones without further demonstration.
Is ISO 3834 compulsory?
The standard itself is voluntary. It becomes binding when a product standard (such as EN 1090-2), a regulation or the contract names it. Where none does, the manufacturer chooses the part using the criteria of part 1.
Who is the welding coordinator under ISO 3834?
The person or team that takes responsibility for the welding in the workshop, with tasks defined in ISO 14731. Required by parts 2 and 3; part 4 sets no specific requirement.