Sections

Site map →

EN

HEA 200 beam: weight per metre and dimensions

HEA 200 weighs 42.3 kg per metre. A 6 m bar is 253.8 kg, a 12 m bar 507.6 kg, and a tonne is about 23.6 m of this section. Nominal values to EN 10365: depth 190 mm, flange width 200 mm.

Mass per metre42.3 kg/m
6 m bar253.8 kg
12 m bar507.6 kg
Metres per tonne23.6 m

Another length or a whole order: the beam weight calculator opens with HEA 200 already selected.

HEA 200 dimensions

DimensionSymbolValue
Depthh190 mm
Flange widthb200 mm
Web thicknesstw6.5 mm
Flange thicknesstf10 mm
Root radiusr18 mm
Cross-section areaA53.8 cm²
Mass per metreG42.3 kg/m

The number in the designation is not the depth: HEA 200 is 190 mm deep with a 200 mm flange. A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEA 200 weight by length

Length, mMass, kg
142.3
284.6
3126.9
4169.2
5211.5
6253.8
8338.4
10423
12507.6

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 507.6 × C and a 6 m bar 253.8 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEA 200 section properties

PropertySymbolValue
Second moment of area, major axisIy3692 cm⁴
Elastic section modulus, major axisWel,y388.6 cm³
Radius of gyration, major axisiy8.28 cm
Second moment of area, minor axisIz1335 cm⁴
Elastic section modulus, minor axisWel,z133.5 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.8: in vertical bending the section is 2.8 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEA 200 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEA 18017118035.52510
HEA 20019020042.33692
HEA 22021022050.55409
IPE 20020010022.41943
HEB 20020020061.35696
UPN 2002007525.31910

Against HEA 200 at the same number: IPE 200 — mass ×0.5, Iy ×0.5; HEB 200 — mass ×1.4, Iy ×1.5; UPN 200 — mass ×0.6, Iy ×0.5. One size up, HEA 220 adds 19 % mass and 47 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEA 200 weigh?

HEA 200 weighs 42.3 kg/m, so a 6 m bar is 253.8 kg and a 12 m bar 507.6 kg. Ten 12 m bars come to 5076 kg.

Which is heavier: IPE 200, HEA 200, HEB 200 or UPN 200?

Per metre: HEB 200 — 61.3 kg/m (h 200 mm); HEA 200 — 42.3 kg/m (h 190 mm); UPN 200 — 25.3 kg/m (h 200 mm); IPE 200 — 22.4 kg/m (h 200 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 200 mean in HEA 200?

The size in the HE range, not the actual depth: HEA 200 is 190 mm deep with a 200 mm flange. HEA is the light series of wide-flange beams and is shallower than its number; HEB 200 is exactly 200 mm deep.

How many metres of HEA 200 are in a tonne?

23.6 m: 1000 kg / 42.3 kg/m. That is about 3.9 bars of 6 m or 2 bars of 12 m.

Does S235 or S355 steel change the weight of HEA 200?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 53.8 cm² × 0.785 = 42.23 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated:

Advertisement