IPE 100 beam: weight per metre and dimensions

IPE 100 weighs 8.1 kg per metre. A 6 m bar is 48.6 kg, a 12 m bar 97.2 kg, and a tonne is about 123 m of this section. Nominal values to EN 10365: depth 100 mm, flange width 55 mm.

Mass per metre8.1 kg/m
6 m bar48.6 kg
12 m bar97.2 kg
Metres per tonne123 m

Another length or a whole order: the beam weight calculator opens with IPE 100 already selected.

IPE 100 dimensions

DimensionSymbolValue
Depthh100 mm
Flange widthb55 mm
Web thicknesstw4.1 mm
Flange thicknesstf5.7 mm
Root radiusr7 mm
Cross-section areaA10.3 cm²
Mass per metreG8.1 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

IPE 100 weight by length

Length, mMass, kg
18.1
216.2
324.3
432.4
540.5
648.6
864.8
1081
1297.2

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 97.2 × C and a 6 m bar 48.6 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

IPE 100 section properties

PropertySymbolValue
Second moment of area, major axisIy171 cm⁴
Elastic section modulus, major axisWel,y34.2 cm³
Radius of gyration, major axisiy4.07 cm
Second moment of area, minor axisIz15.91 cm⁴
Elastic section modulus, minor axisWel,z5.788 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 10.7: in vertical bending the section is 10.7 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

IPE 100 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
IPE 808046680.13
IPE 100100558.1171
IPE 1201206410.4317.7
HEA 1009610016.7349.2
HEB 10010010020.4449.5
UPN 1001005010.6206

Against IPE 100 at the same number: HEA 100 — mass ×2.1, Iy ×2; HEB 100 — mass ×2.5, Iy ×2.6; UPN 100 — mass ×1.3, Iy ×1.2. One size up, IPE 120 adds 28 % mass and 86 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m IPE 100 weigh?

IPE 100 weighs 8.1 kg/m, so a 6 m bar is 48.6 kg and a 12 m bar 97.2 kg. Ten 12 m bars come to 972 kg.

Which is heavier: IPE 100, HEA 100, HEB 100 or UPN 100?

Per metre: HEB 100 — 20.4 kg/m (h 100 mm); HEA 100 — 16.7 kg/m (h 96 mm); UPN 100 — 10.6 kg/m (h 100 mm); IPE 100 — 8.1 kg/m (h 100 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 100 mean in IPE 100?

The nominal depth in millimetres: IPE 100 is 100 mm deep with a 55 mm flange. The letters give the series: IPE, an I-beam with narrow parallel flanges.

How many metres of IPE 100 are in a tonne?

123 m: 1000 kg / 8.1 kg/m. That is about 20.6 bars of 6 m or 10.3 bars of 12 m.

Does S235 or S355 steel change the weight of IPE 100?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 10.3 cm² × 0.785 = 8.09 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated: