Sections

Site map →

EN

HEB 180 beam: weight per metre and dimensions

HEB 180 weighs 51.2 kg per metre. A 6 m bar is 307.2 kg, a 12 m bar 614.4 kg, and a tonne is about 19.5 m of this section. Nominal values to EN 10365: depth 180 mm, flange width 180 mm.

Mass per metre51.2 kg/m
6 m bar307.2 kg
12 m bar614.4 kg
Metres per tonne19.5 m

Another length or a whole order: the beam weight calculator opens with HEB 180 already selected.

HEB 180 dimensions

DimensionSymbolValue
Depthh180 mm
Flange widthb180 mm
Web thicknesstw8.5 mm
Flange thicknesstf14 mm
Root radiusr15 mm
Cross-section areaA65.3 cm²
Mass per metreG51.2 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEB 180 weight by length

Length, mMass, kg
151.2
2102.4
3153.6
4204.8
5256
6307.2
8409.6
10512
12614.4

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 614.4 × C and a 6 m bar 307.2 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEB 180 section properties

PropertySymbolValue
Second moment of area, major axisIy3831 cm⁴
Elastic section modulus, major axisWel,y425.6 cm³
Radius of gyration, major axisiy7.66 cm
Second moment of area, minor axisIz1362 cm⁴
Elastic section modulus, minor axisWel,z151.4 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.8: in vertical bending the section is 2.8 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEB 180 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEB 16016016042.62491
HEB 18018018051.23831
HEB 20020020061.35696
IPE 1801809118.81316
HEA 18017118035.52510
UPN 18018070221350

Against HEB 180 at the same number: IPE 180 — mass ×0.4, Iy ×0.3; HEA 180 — mass ×0.7, Iy ×0.7; UPN 180 — mass ×0.4, Iy ×0.4. One size up, HEB 200 adds 20 % mass and 49 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEB 180 weigh?

HEB 180 weighs 51.2 kg/m, so a 6 m bar is 307.2 kg and a 12 m bar 614.4 kg. Ten 12 m bars come to 6144 kg.

Which is heavier: IPE 180, HEA 180, HEB 180 or UPN 180?

Per metre: HEB 180 — 51.2 kg/m (h 180 mm); HEA 180 — 35.5 kg/m (h 171 mm); UPN 180 — 22 kg/m (h 180 mm); IPE 180 — 18.8 kg/m (h 180 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 180 mean in HEB 180?

The nominal depth in millimetres: HEB 180 is 180 mm deep with a 180 mm flange. The letters give the series: HEB, a standard wide-flange beam.

How many metres of HEB 180 are in a tonne?

19.5 m: 1000 kg / 51.2 kg/m. That is about 3.3 bars of 6 m or 1.6 bars of 12 m.

Does S235 or S355 steel change the weight of HEB 180?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 65.3 cm² × 0.785 = 51.26 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated:

Advertisement