HEB 100 beam: weight per metre and dimensions

HEB 100 weighs 20.4 kg per metre. A 6 m bar is 122.4 kg, a 12 m bar 244.8 kg, and a tonne is about 49 m of this section. Nominal values to EN 10365: depth 100 mm, flange width 100 mm.

Mass per metre20.4 kg/m
6 m bar122.4 kg
12 m bar244.8 kg
Metres per tonne49 m

Another length or a whole order: the beam weight calculator opens with HEB 100 already selected.

HEB 100 dimensions

DimensionSymbolValue
Depthh100 mm
Flange widthb100 mm
Web thicknesstw6 mm
Flange thicknesstf10 mm
Root radiusr12 mm
Cross-section areaA26 cm²
Mass per metreG20.4 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEB 100 weight by length

Length, mMass, kg
120.4
240.8
361.2
481.6
5102
6122.4
8163.2
10204
12244.8

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 244.8 × C and a 6 m bar 122.4 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEB 100 section properties

PropertySymbolValue
Second moment of area, major axisIy449.5 cm⁴
Elastic section modulus, major axisWel,y89.9 cm³
Radius of gyration, major axisiy4.16 cm
Second moment of area, minor axisIz167.2 cm⁴
Elastic section modulus, minor axisWel,z33.45 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.7: in vertical bending the section is 2.7 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEB 100 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEB 10010010020.4449.5
HEB 12012012026.7864.3
IPE 100100558.1171
HEA 1009610016.7349.2
UPN 1001005010.6206

Against HEB 100 at the same number: IPE 100 — mass ×0.4, Iy ×0.4; HEA 100 — mass ×0.8, Iy ×0.8; UPN 100 — mass ×0.5, Iy ×0.5. One size up, HEB 120 adds 31 % mass and 92 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEB 100 weigh?

HEB 100 weighs 20.4 kg/m, so a 6 m bar is 122.4 kg and a 12 m bar 244.8 kg. Ten 12 m bars come to 2448 kg.

Which is heavier: IPE 100, HEA 100, HEB 100 or UPN 100?

Per metre: HEB 100 — 20.4 kg/m (h 100 mm); HEA 100 — 16.7 kg/m (h 96 mm); UPN 100 — 10.6 kg/m (h 100 mm); IPE 100 — 8.1 kg/m (h 100 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 100 mean in HEB 100?

The nominal depth in millimetres: HEB 100 is 100 mm deep with a 100 mm flange. The letters give the series: HEB, a standard wide-flange beam.

How many metres of HEB 100 are in a tonne?

49 m: 1000 kg / 20.4 kg/m. That is about 8.2 bars of 6 m or 4.1 bars of 12 m.

Does S235 or S355 steel change the weight of HEB 100?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 26 cm² × 0.785 = 20.41 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated: