UPN 260 weighs 37.9 kg per metre. A 6 m bar is 227.4 kg, a 12 m bar 454.8 kg, and a tonne is about 26.4 m of this section. Nominal values to DIN 1026-1: depth 260 mm, flange width 90 mm.

Mass per metre37.9 kg/m
6 m bar227.4 kg
12 m bar454.8 kg
Metres per tonne26.4 m

Another length or a whole order: the channel weight calculator opens with UPN 260 already selected.

UPN 260 dimensions

DimensionSymbolValue
Depthh260 mm
Flange widthb90 mm
Web thicknesstw10 mm
Flange thicknesstf14 mm
Root radiusr14 mm
Cross-section areaA48.3 cm²
Mass per metreG37.9 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10279; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

UPN 260 weight by length

Length, mMass, kg
137.9
275.8
3113.7
4151.6
5189.5
6227.4
8303.2
10379
12454.8

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 454.8 × C and a 6 m bar 227.4 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

UPN 260 section properties

PropertySymbolValue
Second moment of area, major axisIy4820 cm⁴
Elastic section modulus, major axisWel,y371 cm³
Radius of gyration, major axisiy9.99 cm
Second moment of area, minor axisIz317 cm⁴
Elastic section modulus, minor axis, at the flange tipWel,z47.7 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 15.2: in vertical bending the section is 15.2 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

UPN 260 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
UPN 2402408533.23600
UPN 2602609037.94820
UPN 2802809541.86280
HEA 26025026068.210450
HEB 2602602609314910

Against UPN 260 at the same number: HEA 260 — mass ×1.8, Iy ×2.2; HEB 260 — mass ×2.5, Iy ×3.1. One size up, UPN 280 adds 10 % mass and 30 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m UPN 260 weigh?

UPN 260 weighs 37.9 kg/m, so a 6 m bar is 227.4 kg and a 12 m bar 454.8 kg. Ten 12 m bars come to 4548 kg.

Which is heavier: HEA 260, HEB 260 or UPN 260?

Per metre: HEB 260 — 93 kg/m (h 260 mm); HEA 260 — 68.2 kg/m (h 250 mm); UPN 260 — 37.9 kg/m (h 260 mm). UPN is a channel and is not symmetric about its web — a different member for different jobs, compared here by weight only.

What does 260 mean in UPN 260?

The nominal depth in millimetres: UPN 260 is 260 mm deep with a 90 mm flange. The letters give the series: UPN, a channel with tapered flanges.

How many metres of UPN 260 are in a tonne?

26.4 m: 1000 kg / 37.9 kg/m. That is about 4.4 bars of 6 m or 2.2 bars of 12 m.

Does S235 or S355 steel change the weight of UPN 260?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 48.3 cm² × 0.785 = 37.92 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10279.

Author: , welder and metal fabricator Updated:

Advertisement