UPN 300 channel: weight per metre and dimensions
UPN 300 weighs 46.2 kg per metre. A 6 m bar is 277.2 kg, a 12 m bar 554.4 kg, and a tonne is about 21.6 m of this section. Nominal values to DIN 1026-1: depth 300 mm, flange width 100 mm.
Another length or a whole order: the channel weight calculator opens with UPN 300 already selected.
UPN 300 dimensions
| Dimension | Symbol | Value |
|---|---|---|
| Depth | h | 300 mm |
| Flange width | b | 100 mm |
| Web thickness | tw | 10 mm |
| Flange thickness | tf | 16 mm |
| Root radius | r | 16 mm |
| Cross-section area | A | 58.8 cm² |
| Mass per metre | G | 46.2 kg/m |
A delivered bar may differ from these nominal values within the rolling tolerances of EN 10279; invoicing goes by the mill certificate, not by the table.

UPN 300 weight by length
| Length, m | Mass, kg |
|---|---|
| 1 | 46.2 |
| 2 | 92.4 |
| 3 | 138.6 |
| 4 | 184.8 |
| 5 | 231 |
| 6 | 277.2 |
| 8 | 369.6 |
| 10 | 462 |
| 12 | 554.4 |
Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 554.4 × C and a 6 m bar 277.2 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.
UPN 300 section properties
| Property | Symbol | Value |
|---|---|---|
| Second moment of area, major axis | Iy | 8030 cm⁴ |
| Elastic section modulus, major axis | Wel,y | 535 cm³ |
| Radius of gyration, major axis | iy | 11.7 cm |
| Second moment of area, minor axis | Iz | 495 cm⁴ |
| Elastic section modulus, minor axis, at the flange tip | Wel,z | 67.8 cm³ |
Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 16.2: in vertical bending the section is 16.2 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.
UPN 300 next to neighbouring sizes
| Section | h, mm | b, mm | kg/m | Iy, cm⁴ |
|---|---|---|---|---|
| UPN 280 | 280 | 95 | 41.8 | 6280 |
| UPN 300 | 300 | 100 | 46.2 | 8030 |
| UPN 350 | 350 | 100 | 60.6 | 12840 |
| IPE 300 | 300 | 150 | 42.2 | 8356 |
| HEA 300 | 290 | 300 | 88.3 | 18260 |
| HEB 300 | 300 | 300 | 117 | 25160 |
Against UPN 300 at the same number: IPE 300 — mass ×0.9, Iy ×1; HEA 300 — mass ×1.9, Iy ×2.3; HEB 300 — mass ×2.5, Iy ×3.1. One size up, UPN 350 adds 31 % mass and 60 % Iy.
Other sizes
- IPE beams: IPE 100 · IPE 120 · IPE 140 · IPE 160 · IPE 180 · IPE 200 · IPE 220 · IPE 240 · IPE 270 · IPE 300
- HEA beams: HEA 100 · HEA 120 · HEA 140 · HEA 160 · HEA 180 · HEA 200 · HEA 220 · HEA 240 · HEA 260 · HEA 280 · HEA 300
- HEB beams: HEB 100 · HEB 120 · HEB 140 · HEB 160 · HEB 180 · HEB 200 · HEB 220 · HEB 240 · HEB 260 · HEB 280 · HEB 300
- UPN channels: UPN 100 · UPN 120 · UPN 140 · UPN 160 · UPN 180 · UPN 200 · UPN 220 · UPN 240 · UPN 260 · UPN 280 · UPN 300
Frequently asked questions
How much does a 6 m and a 12 m UPN 300 weigh?
UPN 300 weighs 46.2 kg/m, so a 6 m bar is 277.2 kg and a 12 m bar 554.4 kg. Ten 12 m bars come to 5544 kg.
Which is heavier: IPE 300, HEA 300, HEB 300 or UPN 300?
Per metre: HEB 300 — 117 kg/m (h 300 mm); HEA 300 — 88.3 kg/m (h 290 mm); UPN 300 — 46.2 kg/m (h 300 mm); IPE 300 — 42.2 kg/m (h 300 mm). UPN is a channel and is not symmetric about its web — a different member for different jobs, compared here by weight only.
What does 300 mean in UPN 300?
The nominal depth in millimetres: UPN 300 is 300 mm deep with a 100 mm flange. The letters give the series: UPN, a channel with tapered flanges.
How many metres of UPN 300 are in a tonne?
21.6 m: 1000 kg / 46.2 kg/m. That is about 3.6 bars of 6 m or 1.8 bars of 12 m.
Does S235 or S355 steel change the weight of UPN 300?
No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 58.8 cm² × 0.785 = 46.16 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10279.
Updated: