UPN 240 channel: weight per metre and dimensions

UPN 240 weighs 33.2 kg per metre. A 6 m bar is 199.2 kg, a 12 m bar 398.4 kg, and a tonne is about 30.1 m of this section. Nominal values to DIN 1026-1: depth 240 mm, flange width 85 mm.

Mass per metre33.2 kg/m
6 m bar199.2 kg
12 m bar398.4 kg
Metres per tonne30.1 m

Another length or a whole order: the channel weight calculator opens with UPN 240 already selected.

UPN 240 dimensions

DimensionSymbolValue
Depthh240 mm
Flange widthb85 mm
Web thicknesstw9.5 mm
Flange thicknesstf13 mm
Root radiusr13 mm
Cross-section areaA42.3 cm²
Mass per metreG33.2 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10279; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

UPN 240 weight by length

Length, mMass, kg
133.2
266.4
399.6
4132.8
5166
6199.2
8265.6
10332
12398.4

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 398.4 × C and a 6 m bar 199.2 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

UPN 240 section properties

PropertySymbolValue
Second moment of area, major axisIy3600 cm⁴
Elastic section modulus, major axisWel,y300 cm³
Radius of gyration, major axisiy9.23 cm
Second moment of area, minor axisIz248 cm⁴
Elastic section modulus, minor axis, at the flange tipWel,z39.6 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 14.5: in vertical bending the section is 14.5 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

UPN 240 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
UPN 2202208029.42690
UPN 2402408533.23600
UPN 2602609037.94820
IPE 24024012030.73891
HEA 24023024060.37763
HEB 24024024083.211250

Against UPN 240 at the same number: IPE 240 — mass ×0.9, Iy ×1.1; HEA 240 — mass ×1.8, Iy ×2.2; HEB 240 — mass ×2.5, Iy ×3.1. One size up, UPN 260 adds 14 % mass and 34 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m UPN 240 weigh?

UPN 240 weighs 33.2 kg/m, so a 6 m bar is 199.2 kg and a 12 m bar 398.4 kg. Ten 12 m bars come to 3984 kg.

Which is heavier: IPE 240, HEA 240, HEB 240 or UPN 240?

Per metre: HEB 240 — 83.2 kg/m (h 240 mm); HEA 240 — 60.3 kg/m (h 230 mm); UPN 240 — 33.2 kg/m (h 240 mm); IPE 240 — 30.7 kg/m (h 240 mm). UPN is a channel and is not symmetric about its web — a different member for different jobs, compared here by weight only.

What does 240 mean in UPN 240?

The nominal depth in millimetres: UPN 240 is 240 mm deep with a 85 mm flange. The letters give the series: UPN, a channel with tapered flanges.

How many metres of UPN 240 are in a tonne?

30.1 m: 1000 kg / 33.2 kg/m. That is about 5 bars of 6 m or 2.5 bars of 12 m.

Does S235 or S355 steel change the weight of UPN 240?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 42.3 cm² × 0.785 = 33.21 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10279.