UPN 280 channel: weight per metre and dimensions

UPN 280 weighs 41.8 kg per metre. A 6 m bar is 250.8 kg, a 12 m bar 501.6 kg, and a tonne is about 23.9 m of this section. Nominal values to DIN 1026-1: depth 280 mm, flange width 95 mm.

Mass per metre41.8 kg/m
6 m bar250.8 kg
12 m bar501.6 kg
Metres per tonne23.9 m

Another length or a whole order: the channel weight calculator opens with UPN 280 already selected.

UPN 280 dimensions

DimensionSymbolValue
Depthh280 mm
Flange widthb95 mm
Web thicknesstw10 mm
Flange thicknesstf15 mm
Root radiusr15 mm
Cross-section areaA53.3 cm²
Mass per metreG41.8 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10279; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

UPN 280 weight by length

Length, mMass, kg
141.8
283.6
3125.4
4167.2
5209
6250.8
8334.4
10418
12501.6

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 501.6 × C and a 6 m bar 250.8 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

UPN 280 section properties

PropertySymbolValue
Second moment of area, major axisIy6280 cm⁴
Elastic section modulus, major axisWel,y448 cm³
Radius of gyration, major axisiy10.9 cm
Second moment of area, minor axisIz399 cm⁴
Elastic section modulus, minor axis, at the flange tipWel,z57.2 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 15.7: in vertical bending the section is 15.7 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

UPN 280 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
UPN 2602609037.94820
UPN 2802809541.86280
UPN 30030010046.28030
HEA 28027028076.413670
HEB 28028028010319270

Against UPN 280 at the same number: HEA 280 — mass ×1.8, Iy ×2.2; HEB 280 — mass ×2.5, Iy ×3.1. One size up, UPN 300 adds 11 % mass and 28 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m UPN 280 weigh?

UPN 280 weighs 41.8 kg/m, so a 6 m bar is 250.8 kg and a 12 m bar 501.6 kg. Ten 12 m bars come to 5016 kg.

Which is heavier: HEA 280, HEB 280 or UPN 280?

Per metre: HEB 280 — 103 kg/m (h 280 mm); HEA 280 — 76.4 kg/m (h 270 mm); UPN 280 — 41.8 kg/m (h 280 mm). UPN is a channel and is not symmetric about its web — a different member for different jobs, compared here by weight only.

What does 280 mean in UPN 280?

The nominal depth in millimetres: UPN 280 is 280 mm deep with a 95 mm flange. The letters give the series: UPN, a channel with tapered flanges.

How many metres of UPN 280 are in a tonne?

23.9 m: 1000 kg / 41.8 kg/m. That is about 4 bars of 6 m or 2 bars of 12 m.

Does S235 or S355 steel change the weight of UPN 280?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 53.3 cm² × 0.785 = 41.84 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10279.