UPN 140 channel: weight per metre and dimensions

UPN 140 weighs 16 kg per metre. A 6 m bar is 96 kg, a 12 m bar 192 kg, and a tonne is about 62.5 m of this section. Nominal values to DIN 1026-1: depth 140 mm, flange width 60 mm.

Mass per metre16 kg/m
6 m bar96 kg
12 m bar192 kg
Metres per tonne62.5 m

Another length or a whole order: the channel weight calculator opens with UPN 140 already selected.

UPN 140 dimensions

DimensionSymbolValue
Depthh140 mm
Flange widthb60 mm
Web thicknesstw7 mm
Flange thicknesstf10 mm
Root radiusr10 mm
Cross-section areaA20.4 cm²
Mass per metreG16 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10279; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

UPN 140 weight by length

Length, mMass, kg
116
232
348
464
580
696
8128
10160
12192

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 192 × C and a 6 m bar 96 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

UPN 140 section properties

PropertySymbolValue
Second moment of area, major axisIy605 cm⁴
Elastic section modulus, major axisWel,y86.4 cm³
Radius of gyration, major axisiy5.45 cm
Second moment of area, minor axisIz62.7 cm⁴
Elastic section modulus, minor axis, at the flange tipWel,z14.8 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 9.6: in vertical bending the section is 9.6 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

UPN 140 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
UPN 1201205513.4364
UPN 1401406016605
UPN 1601606518.8925
IPE 1401407312.9541.2
HEA 14013314024.71033
HEB 14014014033.71509

Against UPN 140 at the same number: IPE 140 — mass ×0.8, Iy ×0.9; HEA 140 — mass ×1.5, Iy ×1.7; HEB 140 — mass ×2.1, Iy ×2.5. One size up, UPN 160 adds 18 % mass and 53 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m UPN 140 weigh?

UPN 140 weighs 16 kg/m, so a 6 m bar is 96 kg and a 12 m bar 192 kg. Ten 12 m bars come to 1920 kg.

Which is heavier: IPE 140, HEA 140, HEB 140 or UPN 140?

Per metre: HEB 140 — 33.7 kg/m (h 140 mm); HEA 140 — 24.7 kg/m (h 133 mm); UPN 140 — 16 kg/m (h 140 mm); IPE 140 — 12.9 kg/m (h 140 mm). UPN is a channel and is not symmetric about its web — a different member for different jobs, compared here by weight only.

What does 140 mean in UPN 140?

The nominal depth in millimetres: UPN 140 is 140 mm deep with a 60 mm flange. The letters give the series: UPN, a channel with tapered flanges.

How many metres of UPN 140 are in a tonne?

62.5 m: 1000 kg / 16 kg/m. That is about 10.4 bars of 6 m or 5.2 bars of 12 m.

Does S235 or S355 steel change the weight of UPN 140?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 20.4 cm² × 0.785 = 16.01 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10279.