Sections

Site map →

EN

HEB 240 beam: weight per metre and dimensions

HEB 240 weighs 83.2 kg per metre. A 6 m bar is 499.2 kg, a 12 m bar 998.4 kg, and a tonne is about 12 m of this section. Nominal values to EN 10365: depth 240 mm, flange width 240 mm.

Mass per metre83.2 kg/m
6 m bar499.2 kg
12 m bar998.4 kg
Metres per tonne12 m

Another length or a whole order: the beam weight calculator opens with HEB 240 already selected.

HEB 240 dimensions

DimensionSymbolValue
Depthh240 mm
Flange widthb240 mm
Web thicknesstw10 mm
Flange thicknesstf17 mm
Root radiusr21 mm
Cross-section areaA106 cm²
Mass per metreG83.2 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEB 240 weight by length

Length, mMass, kg
183.2
2166.4
3249.6
4332.8
5416
6499.2
8665.6
10832
12998.4

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 998.4 × C and a 6 m bar 499.2 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEB 240 section properties

PropertySymbolValue
Second moment of area, major axisIy11250 cm⁴
Elastic section modulus, major axisWel,y938.2 cm³
Radius of gyration, major axisiy10.3 cm
Second moment of area, minor axisIz3922 cm⁴
Elastic section modulus, minor axisWel,z326.8 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.9: in vertical bending the section is 2.9 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEB 240 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEB 22022022071.58090
HEB 24024024083.211250
HEB 2602602609314910
IPE 24024012030.73891
HEA 24023024060.37763
UPN 2402408533.23600

Against HEB 240 at the same number: IPE 240 — mass ×0.4, Iy ×0.3; HEA 240 — mass ×0.7, Iy ×0.7; UPN 240 — mass ×0.4, Iy ×0.3. One size up, HEB 260 adds 12 % mass and 33 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEB 240 weigh?

HEB 240 weighs 83.2 kg/m, so a 6 m bar is 499.2 kg and a 12 m bar 998.4 kg. Ten 12 m bars come to 9984 kg.

Which is heavier: IPE 240, HEA 240, HEB 240 or UPN 240?

Per metre: HEB 240 — 83.2 kg/m (h 240 mm); HEA 240 — 60.3 kg/m (h 230 mm); UPN 240 — 33.2 kg/m (h 240 mm); IPE 240 — 30.7 kg/m (h 240 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 240 mean in HEB 240?

The nominal depth in millimetres: HEB 240 is 240 mm deep with a 240 mm flange. The letters give the series: HEB, a standard wide-flange beam.

How many metres of HEB 240 are in a tonne?

12 m: 1000 kg / 83.2 kg/m. That is about 2 bars of 6 m or 1 bars of 12 m.

Does S235 or S355 steel change the weight of HEB 240?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 106 cm² × 0.785 = 83.21 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated: