HEB 220 beam: weight per metre and dimensions

HEB 220 weighs 71.5 kg per metre. A 6 m bar is 429 kg, a 12 m bar 858 kg, and a tonne is about 14 m of this section. Nominal values to EN 10365: depth 220 mm, flange width 220 mm.

Mass per metre71.5 kg/m
6 m bar429 kg
12 m bar858 kg
Metres per tonne14 m

Another length or a whole order: the beam weight calculator opens with HEB 220 already selected.

HEB 220 dimensions

DimensionSymbolValue
Depthh220 mm
Flange widthb220 mm
Web thicknesstw9.5 mm
Flange thicknesstf16 mm
Root radiusr18 mm
Cross-section areaA91 cm²
Mass per metreG71.5 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEB 220 weight by length

Length, mMass, kg
171.5
2143
3214.5
4286
5357.5
6429
8572
10715
12858

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 858 × C and a 6 m bar 429 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEB 220 section properties

PropertySymbolValue
Second moment of area, major axisIy8090 cm⁴
Elastic section modulus, major axisWel,y735.5 cm³
Radius of gyration, major axisiy9.43 cm
Second moment of area, minor axisIz2843 cm⁴
Elastic section modulus, minor axisWel,z258.4 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.8: in vertical bending the section is 2.8 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEB 220 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEB 20020020061.35696
HEB 22022022071.58090
HEB 24024024083.211250
IPE 22022011026.22771
HEA 22021022050.55409
UPN 2202208029.42690

Against HEB 220 at the same number: IPE 220 — mass ×0.4, Iy ×0.3; HEA 220 — mass ×0.7, Iy ×0.7; UPN 220 — mass ×0.4, Iy ×0.3. One size up, HEB 240 adds 16 % mass and 39 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEB 220 weigh?

HEB 220 weighs 71.5 kg/m, so a 6 m bar is 429 kg and a 12 m bar 858 kg. Ten 12 m bars come to 8580 kg.

Which is heavier: IPE 220, HEA 220, HEB 220 or UPN 220?

Per metre: HEB 220 — 71.5 kg/m (h 220 mm); HEA 220 — 50.5 kg/m (h 210 mm); UPN 220 — 29.4 kg/m (h 220 mm); IPE 220 — 26.2 kg/m (h 220 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 220 mean in HEB 220?

The nominal depth in millimetres: HEB 220 is 220 mm deep with a 220 mm flange. The letters give the series: HEB, a standard wide-flange beam.

How many metres of HEB 220 are in a tonne?

14 m: 1000 kg / 71.5 kg/m. That is about 2.3 bars of 6 m or 1.2 bars of 12 m.

Does S235 or S355 steel change the weight of HEB 220?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 91 cm² × 0.785 = 71.44 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated: