HEB 140 beam: weight per metre and dimensions

HEB 140 weighs 33.7 kg per metre. A 6 m bar is 202.2 kg, a 12 m bar 404.4 kg, and a tonne is about 29.7 m of this section. Nominal values to EN 10365: depth 140 mm, flange width 140 mm.

Mass per metre33.7 kg/m
6 m bar202.2 kg
12 m bar404.4 kg
Metres per tonne29.7 m

Another length or a whole order: the beam weight calculator opens with HEB 140 already selected.

HEB 140 dimensions

DimensionSymbolValue
Depthh140 mm
Flange widthb140 mm
Web thicknesstw7 mm
Flange thicknesstf12 mm
Root radiusr12 mm
Cross-section areaA43 cm²
Mass per metreG33.7 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEB 140 weight by length

Length, mMass, kg
133.7
267.4
3101.1
4134.8
5168.5
6202.2
8269.6
10337
12404.4

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 404.4 × C and a 6 m bar 202.2 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEB 140 section properties

PropertySymbolValue
Second moment of area, major axisIy1509 cm⁴
Elastic section modulus, major axisWel,y215.6 cm³
Radius of gyration, major axisiy5.92 cm
Second moment of area, minor axisIz549.6 cm⁴
Elastic section modulus, minor axisWel,z78.52 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.7: in vertical bending the section is 2.7 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEB 140 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEB 12012012026.7864.3
HEB 14014014033.71509
HEB 16016016042.62491
IPE 1401407312.9541.2
HEA 14013314024.71033
UPN 1401406016605

Against HEB 140 at the same number: IPE 140 — mass ×0.4, Iy ×0.4; HEA 140 — mass ×0.7, Iy ×0.7; UPN 140 — mass ×0.5, Iy ×0.4. One size up, HEB 160 adds 26 % mass and 65 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEB 140 weigh?

HEB 140 weighs 33.7 kg/m, so a 6 m bar is 202.2 kg and a 12 m bar 404.4 kg. Ten 12 m bars come to 4044 kg.

Which is heavier: IPE 140, HEA 140, HEB 140 or UPN 140?

Per metre: HEB 140 — 33.7 kg/m (h 140 mm); HEA 140 — 24.7 kg/m (h 133 mm); UPN 140 — 16 kg/m (h 140 mm); IPE 140 — 12.9 kg/m (h 140 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 140 mean in HEB 140?

The nominal depth in millimetres: HEB 140 is 140 mm deep with a 140 mm flange. The letters give the series: HEB, a standard wide-flange beam.

How many metres of HEB 140 are in a tonne?

29.7 m: 1000 kg / 33.7 kg/m. That is about 4.9 bars of 6 m or 2.5 bars of 12 m.

Does S235 or S355 steel change the weight of HEB 140?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 43 cm² × 0.785 = 33.76 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated: