Sections

Site map →

EN

UPN 200 channel: weight per metre and dimensions

UPN 200 weighs 25.3 kg per metre. A 6 m bar is 151.8 kg, a 12 m bar 303.6 kg, and a tonne is about 39.5 m of this section. Nominal values to DIN 1026-1: depth 200 mm, flange width 75 mm.

Mass per metre25.3 kg/m
6 m bar151.8 kg
12 m bar303.6 kg
Metres per tonne39.5 m

Another length or a whole order: the channel weight calculator opens with UPN 200 already selected.

UPN 200 dimensions

DimensionSymbolValue
Depthh200 mm
Flange widthb75 mm
Web thicknesstw8.5 mm
Flange thicknesstf11.5 mm
Root radiusr—
Cross-section areaA32.2 cm²
Mass per metreG25.3 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10279; invoicing goes by the mill certificate, not by the table. “—”: the sources give r for this size to different precision.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

UPN 200 weight by length

Length, mMass, kg
125.3
250.6
375.9
4101.2
5126.5
6151.8
8202.4
10253
12303.6

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 303.6 × C and a 6 m bar 151.8 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

UPN 200 section properties

PropertySymbolValue
Second moment of area, major axisIy1910 cm⁴
Elastic section modulus, major axisWel,y191 cm³
Radius of gyration, major axisiy7.70 cm
Second moment of area, minor axisIz148 cm⁴
Elastic section modulus, minor axis, at the flange tipWel,z27 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 12.9: in vertical bending the section is 12.9 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

UPN 200 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
UPN 18018070221350
UPN 2002007525.31910
UPN 2202208029.42690
IPE 20020010022.41943
HEA 20019020042.33692
HEB 20020020061.35696

Against UPN 200 at the same number: IPE 200 — mass ×0.9, Iy ×1; HEA 200 — mass ×1.7, Iy ×1.9; HEB 200 — mass ×2.4, Iy ×3. One size up, UPN 220 adds 16 % mass and 41 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m UPN 200 weigh?

UPN 200 weighs 25.3 kg/m, so a 6 m bar is 151.8 kg and a 12 m bar 303.6 kg. Ten 12 m bars come to 3036 kg.

Which is heavier: IPE 200, HEA 200, HEB 200 or UPN 200?

Per metre: HEB 200 — 61.3 kg/m (h 200 mm); HEA 200 — 42.3 kg/m (h 190 mm); UPN 200 — 25.3 kg/m (h 200 mm); IPE 200 — 22.4 kg/m (h 200 mm). UPN is a channel and is not symmetric about its web — a different member for different jobs, compared here by weight only.

What does 200 mean in UPN 200?

The nominal depth in millimetres: UPN 200 is 200 mm deep with a 75 mm flange. The letters give the series: UPN, a channel with tapered flanges.

How many metres of UPN 200 are in a tonne?

39.5 m: 1000 kg / 25.3 kg/m. That is about 6.6 bars of 6 m or 3.3 bars of 12 m.

Does S235 or S355 steel change the weight of UPN 200?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 32.2 cm² × 0.785 = 25.28 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10279.

Author: , welder and metal fabricator Updated:

Advertisement