IPE 140 beam: weight per metre and dimensions

IPE 140 weighs 12.9 kg per metre. A 6 m bar is 77.4 kg, a 12 m bar 154.8 kg, and a tonne is about 77.5 m of this section. Nominal values to EN 10365: depth 140 mm, flange width 73 mm.

Mass per metre12.9 kg/m
6 m bar77.4 kg
12 m bar154.8 kg
Metres per tonne77.5 m

Another length or a whole order: the beam weight calculator opens with IPE 140 already selected.

IPE 140 dimensions

DimensionSymbolValue
Depthh140 mm
Flange widthb73 mm
Web thicknesstw4.7 mm
Flange thicknesstf6.9 mm
Root radiusr7 mm
Cross-section areaA16.4 cm²
Mass per metreG12.9 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

IPE 140 weight by length

Length, mMass, kg
112.9
225.8
338.7
451.6
564.5
677.4
8103.2
10129
12154.8

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 154.8 × C and a 6 m bar 77.4 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

IPE 140 section properties

PropertySymbolValue
Second moment of area, major axisIy541.2 cm⁴
Elastic section modulus, major axisWel,y77.31 cm³
Radius of gyration, major axisiy5.74 cm
Second moment of area, minor axisIz44.91 cm⁴
Elastic section modulus, minor axisWel,z12.3 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 12.1: in vertical bending the section is 12.1 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

IPE 140 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
IPE 1201206410.4317.7
IPE 1401407312.9541.2
IPE 1601608215.8869.2
HEA 14013314024.71033
HEB 14014014033.71509
UPN 1401406016605

Against IPE 140 at the same number: HEA 140 — mass ×1.9, Iy ×1.9; HEB 140 — mass ×2.6, Iy ×2.8; UPN 140 — mass ×1.2, Iy ×1.1. One size up, IPE 160 adds 22 % mass and 61 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m IPE 140 weigh?

IPE 140 weighs 12.9 kg/m, so a 6 m bar is 77.4 kg and a 12 m bar 154.8 kg. Ten 12 m bars come to 1548 kg.

Which is heavier: IPE 140, HEA 140, HEB 140 or UPN 140?

Per metre: HEB 140 — 33.7 kg/m (h 140 mm); HEA 140 — 24.7 kg/m (h 133 mm); UPN 140 — 16 kg/m (h 140 mm); IPE 140 — 12.9 kg/m (h 140 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 140 mean in IPE 140?

The nominal depth in millimetres: IPE 140 is 140 mm deep with a 73 mm flange. The letters give the series: IPE, an I-beam with narrow parallel flanges.

How many metres of IPE 140 are in a tonne?

77.5 m: 1000 kg / 12.9 kg/m. That is about 12.9 bars of 6 m or 6.5 bars of 12 m.

Does S235 or S355 steel change the weight of IPE 140?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 16.4 cm² × 0.785 = 12.87 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.