HEB 160 beam: weight per metre and dimensions

HEB 160 weighs 42.6 kg per metre. A 6 m bar is 255.6 kg, a 12 m bar 511.2 kg, and a tonne is about 23.5 m of this section. Nominal values to EN 10365: depth 160 mm, flange width 160 mm.

Mass per metre42.6 kg/m
6 m bar255.6 kg
12 m bar511.2 kg
Metres per tonne23.5 m

Another length or a whole order: the beam weight calculator opens with HEB 160 already selected.

HEB 160 dimensions

DimensionSymbolValue
Depthh160 mm
Flange widthb160 mm
Web thicknesstw8 mm
Flange thicknesstf13 mm
Root radiusr15 mm
Cross-section areaA54.3 cm²
Mass per metreG42.6 kg/m

A delivered bar may differ from these nominal values within the rolling tolerances of EN 10034; invoicing goes by the mill certificate, not by the table.

Cross-sections of an I-beam, a channel and an angle with dimensions h, b, s and t
In the drawing s is the web thickness (tw) and t the flange thickness (tf)

Download the diagram: SVG · PNG

HEB 160 weight by length

Length, mMass, kg
142.6
285.2
3127.8
4170.4
5213
6255.6
8340.8
10426
12511.2

Steel cost is mass times the price per kilogram: at a price C per kg a 12 m bar costs 511.2 × C and a 6 m bar 255.6 × C. Cutting, drilling and painting are priced separately; paint goes by surface area, not by weight.

Advertisement

HEB 160 section properties

PropertySymbolValue
Second moment of area, major axisIy2491 cm⁴
Elastic section modulus, major axisWel,y311.4 cm³
Radius of gyration, major axisiy6.77 cm
Second moment of area, minor axisIz889.2 cm⁴
Elastic section modulus, minor axisWel,z111.1 cm³

Iy governs deflection, Wel,y bending stress, iy the slenderness of a strut. Iy / Iz = 2.8: in vertical bending the section is 2.8 times stiffer than sideways. Source: ArcelorMittal catalogue “Sections and Merchant Bars” (2023), each value checked against a second, independent table. These are inputs for a check to EN 1993-1-1, not a load capacity.

HEB 160 next to neighbouring sizes

Sectionh, mmb, mmkg/mIy, cm⁴
HEB 14014014033.71509
HEB 16016016042.62491
HEB 18018018051.23831
IPE 1601608215.8869.2
HEA 16015216030.41672
UPN 1601606518.8925

Against HEB 160 at the same number: IPE 160 — mass ×0.4, Iy ×0.3; HEA 160 — mass ×0.7, Iy ×0.7; UPN 160 — mass ×0.4, Iy ×0.4. One size up, HEB 180 adds 20 % mass and 54 % Iy.

Other sizes

Frequently asked questions

How much does a 6 m and a 12 m HEB 160 weigh?

HEB 160 weighs 42.6 kg/m, so a 6 m bar is 255.6 kg and a 12 m bar 511.2 kg. Ten 12 m bars come to 5112 kg.

Which is heavier: IPE 160, HEA 160, HEB 160 or UPN 160?

Per metre: HEB 160 — 42.6 kg/m (h 160 mm); HEA 160 — 30.4 kg/m (h 152 mm); UPN 160 — 18.8 kg/m (h 160 mm); IPE 160 — 15.8 kg/m (h 160 mm). The wide-flange HE sections carry load in both planes and go into columns; IPE is the lighter floor beam for bending in one plane.

What does 160 mean in HEB 160?

The nominal depth in millimetres: HEB 160 is 160 mm deep with a 160 mm flange. The letters give the series: HEB, a standard wide-flange beam.

How many metres of HEB 160 are in a tonne?

23.5 m: 1000 kg / 42.6 kg/m. That is about 3.9 bars of 6 m or 2 bars of 12 m.

Does S235 or S355 steel change the weight of HEB 160?

No. The table mass is the cross-section area times the density of steel, 7850 kg/m³: 54.3 cm² × 0.785 = 42.63 kg/m. The grade to EN 10025-2 sets strength, not density. A real bar differs from nominal only within the rolling tolerances of EN 10034.

Author: , welder and metal fabricator Updated: